High Quality Molecular Sieve 3A Pellet as Adsorbent
Product Introduction
Large water absorption capacity
Strong moisture absorption
The molecular sieve has many channels with uniform pore size and neatly arranged holes in its structure
... …
Fast drying speed
Quick drying
The molecular sieve has uniform pore size distribution, which can play a role in quick drying
… …
Long service life
Long-term use
Can be regenerated under high pressure and high temperature, with long service life
...
High strength
Not easy to break
The raw material is natural zeolite, which is not easy to break
Chemical Molecular Formula: 2/3K2o.1/3na2o.Al2O3.2sio2.9/2H2O
Technical parameters
Item |
Unit |
Target |
Diameter |
mm |
0.5-0.9 |
1.0-1.5 |
1.5-2.0 |
Bulk density |
g/ml |
0.75-0.85 |
0.75-0.85 |
0.75-0.85 |
Size ratio up to grade |
% |
≥98.0 |
≥98.0 |
≥98.0 |
Delta T value |
ºC(10g MS-3A/10ml H2O) |
≥30 |
≥30 |
≥30 |
ºC(50g MS-3A/50ml H2O) |
≥30 |
≥30 |
≥30 |
AWAC |
%(RH9%, 25ºC) |
≥16.0 |
≥16.0 |
≥16.0 |
Nitrogen adsorption |
ml/g (250ml-MS 3A, 70ºC, 4hs) |
≤0.3 |
≤0.3 |
≤0.3 |
Dew point |
ºC |
≤-60 |
≤-60 |
≤-60 |
Dust drops |
NTU |
≤50 |
≤50 |
≤50 |
LOI |
%(540ºC) |
≤1.7 |
≤1.7 |
≤1.7
|
Advantage
1. The high temperature rise value, the temperature rise of molecular sieve exceeds 50ºC (25g molecular sieve/25ml water), which ensures that the insulating glass can last more than 10 years.
2. The extremely low powder falling rate is the biggest advantage of molecular sieve, which fully guarantees the cleanliness of the glass itself and its processing environment.
3. The extremely low water content of the package and strict testing standards determine its extremely low water content. Ensure that the hollow glass is in a low dew point state for a long time (the lower the dew point, the higher the degree of drying, the better the effect of the hollow glass).
4. High water adsorption capacity, especially in the case of low relative humidity, still maintains a strong drying capacity, this feature ensures a long service life of the insulating glass. The higher temperature rise value can also indirectly reflect the situation of this indicator.
5. It is clean and free of debris and dust, and the spherical surface is smooth and broken. This is the result of strict quality control of molecular sieve.
6. The price is reasonable, allowing you to experience the convenience and benefits brought to you by the molecular sieve technology.
Packing and Shipping
Aluminum foil bag
Composed of several layer aluminum foils.
150kg steel drum
Every drum has passed the test for air tightness.
140kg fiber drum
It is made of brown fiber paper. Very strong and environmental.
Big bag
We can offer all sizes of big bags. Tightknit and convenient.
20'GP container can be loaded: 600 cartons, net weight 15000kg or 80 fiber drums, net weight 11200kg; or 80 steel drums, net weight 12000kg. 40'GP container can be loaded:1000 cartons, net weight 25000kg; or 160 fiber drums, net weight 22400kg or 160 steel drums, net weight 24000kg.
Precautions
1. The insulating glass desiccant should be sealed and stored before use. When in use, it should be filled quickly, and the unused molecular sieve should be sealed in time to avoid moisture absorption.
2. Molecular sieve that cannot be determined whether it absorbs moisture should be tested for temperature rise. When the temperature rise is lower than 33 degrees Celsius (25 grams molecular sieve/25 ml water), it cannot be used again and should be recycled by the manufacturer.
3. The manufacturer should have at least two detection methods for temperature rise and molecular sieve desiccant outgassing.